ASTM F3418-20 Standard Test Method for Measurement of Transition Temperatures of Slack Waxes used in Equine Sports Surfaces by Differential Scanning Calorimetry (DSC)
Status
Published
on 23 Apr 2020
Year of Creation
2020
Copyright Claimant
ASTM International
Registration Number
TX0008868993
on 23 Apr 2020Copyright Summary
The U.S. Copyright record (Registration Number: TX0008868993) dated 23 Apr 2020, pertains to an electronic file (eService) titled "ASTM F3418-20 Standard Test Method for Measurement of Transition Temperatures of Slack Waxes used in Equine Sports Surfaces by Differential Scanning Calorimetry (DSC)" created in 2020. The copyright holder is ASTM International, known for their creative contributions in text registration. For any inquiries concerning this copyrighted material, kindly reach out to ASTM International.
Application Details
Registration Number
TX0008868993
Registration Date
4/23/2020
Year of Creation
2020
Agency Marc Code
DLC-CO
Record Status
New
Corporate Author
ASTM International
Physical Description
Electronic file (eService)
First Publication Nation
United States
Notes
Rights Note: Kathleen Hooper, ASTM International, 100 Barr Harbor Drive, West Conshohocken, PA, 19428, United States, (610) 832-9634, khooper@astm.org
Statements
Application Title Statement: ASTM F3418-20 Standard Test Method for Measurement of Transition Temperatures of Slack Waxes used in Equine Sports Surfaces by Differential Scanning Calorimetry (DSC)
Author Statement: ASTM International employer for hire Domicile: United States Authorship: text
© 2025 reserved by Trademarkia
Show terms & conditions
Disclaimer: The information contained in this website is provided for informational purposes only, and should not be construed as legal advice. Although LegalForce RAPC Worldwide P.C., dba Trademarkia P.C., is a law firm (the “Firm”), your use of this website does not establish an attorney-client relationship with the Firm. Such a relationship can only be established after the Firm decides that it is willing and able to accept the engagement after a conflict check and after a written retainer agreement is agreed upon between you and the Firm. Your use of this website is also subject to our Terms of Use and Privacy Policy. ** The entry level subscription is a bundled price which requires a minimum of two billing cycles, or 6 months.